0
RESEARCH PAPERS

External Corrosion of Superheaters in Boilers Firing High-Alkali Coals

[+] Author and Article Information
P. Sedor, E. K. Diehl, D. H. Barnhart

The Babcock & Wilcox Company, Research Center, Alliance, Ohio

J. Eng. Power 82(3), 181-190 (Jul 01, 1960) (10 pages) doi:10.1115/1.3672755 History: Received August 03, 1959; Online January 10, 2012

Abstract

In the past few years, corrosion of high-temperature superheaters and reheaters has become an increasingly serious problem on coal-fired boilers. A type of corrosion that has occurred on several boilers in the Chicago area which burn high-alkali coal is described. The results obtained from an experimental study of the factors influencing the rate of attack and the control measures applied are described.

Copyright © 1960 by ASME
Your Session has timed out. Please sign back in to continue.

References

Figures

Tables

Errata

Discussions

Some tools below are only available to our subscribers or users with an online account.

Related Content

Customize your page view by dragging and repositioning the boxes below.

Related Journal Articles
Related eBook Content
Topic Collections

Sorry! You do not have access to this content. For assistance or to subscribe, please contact us:

  • TELEPHONE: 1-800-843-2763 (Toll-free in the USA)
  • EMAIL: asmedigitalcollection@asme.org
Sign In